The steel angles acid bath is finished and we are ready for the truly dangerous part of the process Good thing my apron is strapped on tight And this is the zinc melted Time now to clean the surface of the molten zinc We're gonna show you in a minute I'm gonna come to the side pick them up and let them drain a little bit and put it right there See all the zinc coming out So what's happening here it's a shovel like a sieve and you're scooping into the zinc and the zinc is dripping out at 850 degrees and the ash stays in sort of and you dump the ash That's the idea Now we're just gonna dip your angles That's what we're shooting for My angles are ready for their zinc bath